Purified Terephthalic Acid

    • Product Name: Purified Terephthalic Acid
    • Factroy Site: Midong District, Urumqi City, Xinjiang Uygur Autonomous Region
    • Price Inquiry: sales7@petrochina-nanjing.com
    • Manufacturer: PetroChina Urumqi Petrochemical Company
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 271936
    Productname Purified Terephthalic Acid
    Abbreviation PTA
    Iupacname benzene-1,4-dicarboxylic acid
    Chemicalformula C8H6O4
    Molecularweight 166.13 g/mol
    Casnumber 100-21-0
    Appearance White crystalline powder
    Purity ≥99.9%
    Meltingpoint >300 °C
    Sublimationpoint 402 °C
    Density 1.51 g/cm³
    Solubilityinwater Practically insoluble, about 15 mg/L at 20 °C
    Acidityconstants pKa1 = 3.51; pKa2 = 4.82
    Odor Odorless

    As an accredited Purified Terephthalic Acid factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Purified Terephthalic Acid supplied in 1,000 kg woven polypropylene jumbo bags with inner polyethylene liner, UV-stabilized, moisture-barrier packaging.
    Container Loading (20′ FCL) 20′ FCL loaded with Purified Terephthalic Acid in bagged/palletized form, securely stowed, sealed, and labelled for safe chemical transport.
    Shipping Purified Terephthalic Acid is typically shipped as a white crystalline powder in 25 kg bags, 500–1,000 kg flexible intermediate bulk containers (FIBCs), or bulk trucks and railcars. Though non-hazardous, it requires dry, clean, covered transport and dust-control measures to prevent moisture, contamination, and combustible dust hazards.
    Storage Store Purified Terephthalic Acid in a cool, dry, well-ventilated area with containers tightly closed. Keep away from ignition sources, heat, and strong oxidizers. Prevent dust generation and accumulation; use explosion-proof equipment and grounding/bonding. Protect from moisture and incompatible substances. Store in original labeled containers, away from food, drink, and animal feed. Follow local regulations and maintain good housekeeping.
    Shelf Life Purified terephthalic acid is highly stable; when stored dry, sealed, and away from heat, it has an indefinite shelf life.
    Application of Purified Terephthalic Acid

    What Limits Carboxy End-Group Formation in Continuous PET Fibre Polymerisation?

    In continuous polyester fibre melt polymerisation based on purified terephthalic acid (CAS 100-21-0), the glycol-to-acid feed ratio is maintained at 1.15:1 to 1.25:1 ethylene glycol per mole PTA, corresponding to a PTA charge of 85.0–87.0 parts by mass per 100 parts final poly(ethylene terephthalate). The slurry contains antimony trioxide at 190–240 mg/kg Sb and phosphoric acid at 15–40 mg/kg P. Esterification in the primary esterifier runs at 260–270 °C and 100–200 kPa absolute, with 2.5–4.0 h residence time; the oligomer reaches a degree of polymerisation of 4–8 and a carboxyl end-group concentration of 15–30 meq/kg. Polycondensation proceeds at 270–285 °C under <100 Pa, producing fibre-grade chips with intrinsic viscosity 0.62–0.68 dL/g measured by ASTM D4603. Plant-scale observation shows that PTA with median particle size above 180 µm increases slurry settling in the esterification feed legs and causes lobe-pump suction pressure oscillation; 20–40 µm spinneret filtration and melt-pump pressure of 8–14 MPa are required to avoid particle-related filament breaks. The melt is extruded through spinnerets, quenched at 0.4–0.7 m/s air velocity, drawn, crimped, and cut. Terminal products include semi-dull staple fibre, fully drawn filament yarn, low-pill fibre, and needle-punched nonwoven. Compliance is anchored to REACH (EC 1907/2006) Article 14 exposure scenarios, OEKO-TEX Standard 100 Annex 4 Class II, and yarn tensile testing per ISO 2062:2009.

    A 600 t/d bottle-resin line processing amorphous copolymer precursor uses a diacid feed containing 1.5–2.5 wt% isophthalic acid and a molar glycol-to-PTA ratio of 1.08:1 to 1.12:1, which places PTA at 84.5–86.5 parts per 100 parts pellet mass after melt-phase losses. The melt-phase finisher discharges resin at intrinsic viscosity 0.60–0.64 dL/g; solid-state polycondensation in a continuous shaft dryer with nitrogen dew point −60 °C, temperature 205–215 °C, and residence time 12–18 h raises intrinsic viscosity to 0.82–0.86 dL/g and lowers pellet acetaldehyde to ≤1 mg/kg. Process constraints include nitrogen flow 4–6 m/s superficial velocity and pellet bed height 1.5–2.2 m to avoid dusting and local overheating. Terminal packaging grades include carbonated soft-drink bottles, hot-fill containers, aseptic dairy packaging, and food trays. The compliance matrix below defines the boundary for food-contact export documentation.

    Regulatory frameDesignationCritical limit / method
    EU food-contact plasticsRegulation (EU) No 10/2011, Annex I, FCM substance No 785PTA specific migration limit 7.5 mg/kg
    US food-contact polymer21 CFR §177.1630PET polymer specification for aqueous and hot-fill food contact
    Residual acetaldehydeASTM F2013-10 headspace GC≤ 3 mg/kg preform for still water

    PBT Direct Esterification: Tetrahydrofuran Loss and Molar Balance Control

    Polybutylene terephthalate is produced from PTA and 1,4-butanediol using a diol-to-PTA molar feed ratio of 1.30:1 to 1.45:1, with PTA representing 56–60 parts per 100 parts raw diol/diacid charge before recovery. The excess diol compensates for dehydration to tetrahydrofuran, which is collected in the overhead decanter and returned after distillation; tetrahydrofuran yield is typically 0.5–1.5 mol% on BDO. Esterification at 225–235 °C is followed by polycondensation at 245–255 °C and <100 Pa with tetrabutyl titanate catalyst at 50–120 mg/kg Ti. Injection-moulding grades exit with intrinsic viscosity 0.95–1.10 dL/g in 60:40 w/w phenol/tetrachloroethane, and melt volume-flow rate 12–18 cm³/10 min at 250 °C/2.16 kg per ISO 1133-1:2022. Reinforced compounds with 30 wt% glass fibre are produced on a L/D 40:1 twin-screw extruder with barrel profile 230–260 °C; tensile stress at break is 130–140 MPa per ISO 527-2. Pre-drying at 120 °C for 4 h to below 0.02 wt% moisture is mandatory; hydrolysis reduces molecular weight by 10–20% after 8 h at 250 °C if moisture exceeds 0.05 wt%. Terminal products include automotive ignition coil bobbins, electrical connectors, sensor housings, and pump rotors. Compliance is based on UL 94 V-0 at 0.75 mm, IEC 60112:2020 comparative tracking index, and ISO 527-2:2012 mechanical data.

    At a 20 m³ jacketed esterification reactor operating with 2-ethylhexanol as the excess alcohol, PTA is metered at 39–43 parts by mass per 100 parts recovered dioctyl terephthalate, with a molar alcohol-to-PTA ratio of 2.20:1 to 2.50:1. The catalyst is tetrabutyl titanate at 0.05–0.15 wt% of PTA; esterification is maintained at 190–220 °C while water is removed as a 2-ethylhexanol azeotrope, returned through an overhead decanter, and the recovered alcohol is recycled. Esterification continues until acid value is below 0.10 mg KOH/g; neutralisation with 0.1–0.3 wt% aqueous sodium carbonate, filtration through 1 µm media, and vacuum stripping at 15–25 kPa reduce moisture to <0.05 wt% and colour to <30 Hazen. In flexible PVC compounding, DOTP is added at 35–70 phr to produce Shore A hardness from 60 to 85; twin-screw compounding at 160–175 °C with a L/D 40:1 configuration provides sufficient dispersion. Terminal products include 80 °C building wire insulation, appliance wire jackets, calender-made vinyl flooring, and artificial leather. DOTP is not listed under REACH Annex XVII Entry 51 restrictions for DEHP, DBP, BBP, and DIBP, and is not restricted under EU RoHS Directive 2011/65/EU Annex II; batch documentation must nevertheless include REACH registration and Prop 65 certification for North American wire exports.

    When PTA Replaces Phthalic Anhydride in Aromatic Polyester Polyol Kettle Processing

    When PTA replaces part of the phthalic anhydride in a batch aromatic polyester polyol cook, the charge is set at 15–45 wt% of the total diacid/diol mass, with diethylene glycol as the main glycol and 5–15 wt% adipic acid or phthalic anhydride as modifier. A 10–20 m³ kettle with a helical ribbon impeller operating at 0.5–1.0 m/s tip speed keeps PTA suspended until dissolution above 180 °C. Reaction proceeds at 220–240 °C under nitrogen with organotin catalyst at 50–100 mg/kg; vacuum is ramped to <500 Pa until acid number reaches 1.5–2.5 mg KOH/g and hydroxyl number is 180–320 mg KOH/g. The finished polyol has viscosity 8,000–15,000 mPa·s at 25 °C and water content <0.05 wt%. In rigid polyurethane foam, a formulation uses 100 parts polyester polyol, 2–4 parts water, 1–3 parts amine catalyst, 1–2 parts silicone surfactant, and polymeric MDI at an isocyanate index of 105–180. Compressive strength by EN 826:2013 is 250–450 kPa for 40–80 kg/m³ core density. Terminal products include laminated boardstock, pour-in-place appliance insulation, spray-applied insulation, and district heating pipe segments. Fire performance is evaluated under ASTM E84-20 Class A/B and EN 13501-1:2018 with flame retardant additions of 5–15 parts depending target Euroclass. PTA-based polyols crystallise below 25 °C; storage at 40–60 °C with recirculation is required to prevent solidification.

    Biaxially oriented polyester film casting begins with a pellet feedstock whose intrinsic viscosity is deliberately raised to 0.65–0.68 dL/g by melt-phase polycondensation from PTA and ethylene glycol at a glycol-to-PTA molar ratio of 1.13:1, equivalent to 85–86 parts PTA per 100 parts final polymer. Film formulations include silica anti-block at 0.05–0.40 wt%, magnesium acetate at 0.03–0.05 wt%, and phosphoric acid at 0.03–0.06 wt%. The melt is filtered through 15 µm media and extruded at 275–285 °C through a slot die onto a casting drum at 20–30 °C. Sequential stretching uses machine-direction draw ratio 3.2–3.8:1 at 90–110 °C and transverse-direction draw ratio 3.5–4.2:1 at 110–130 °C, followed by heat setting at 220–230 °C and 1–3% relaxation. Terminal products include 1.5–6 µm capacitor film with surface roughness 0.030–0.050 µm, 50–250 µm solar backsheet film, 12–50 µm flexible packaging, and 25–125 µm release liner. Mechanical inspection uses ASTM D882-18 tensile stress 200–250 MPa in both directions, ASTM D1003-21 haze below 3%, and IEC 60674-3 film specifications. Food-contact status is governed by 21 CFR §177.1630 and Regulation (EU) No 10/2011; hydrolysis-resistant grades require 0.5–1.0 wt% carbodiimide-based stabiliser for extended thermal cycling in photovoltaic modules. Published data for specific capacitor-grade monolayer PTA-based PET from individual lines is limited; the cited ranges reflect equipment manufacturer technical bulletins and film-converter specifications.

    Related Articles
    Free Quote

    Competitive Purified Terephthalic Acid prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615371019725 or mail to sales7@petrochina-nanjing.com.

    We will respond to you as soon as possible.

    Tel: +8615371019725

    Email: sales7@petrochina-nanjing.com

    Inquiry

    Get Free Quote of PetroChina Urumqi Petrochemical Company

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Purified Terephthalic Acid (PTA; CAS 100-21-0) is the aromatic dicarboxylic acid derived from catalytic air oxidation of p-xylene and used as the primary terephthaloyl monomer in melt-phase polyethylene terephthalate (PET) polymerisation. Its molecular formula is C8H6O4, with a molecular weight of 166.13 g/mol and a theoretical acid number of 675–677 mg KOH/g. The polyester-grade model, commonly designated as “PTA polyester grade” in supplier documentation, is distinguished from crude terephthalic acid and medium-purity terephthalic acid by controlled residual aldehyde content, monofunctional aromatic acid content, transition-metal ash, and colour coordinates. Typical bulk density ranges from 800–1,000 kg/m3, and the product is handled as a free-flowing white crystalline powder. The primary downstream application is continuous and batch production of PET homopolymers and copolymers for bottle resin, textile fibre, film, and specialty polyester applications. The specification boundaries, process sensitivities, and product comparisons required for material selection are detailed below.

    What Purification Thresholds Separate Polyester-Grade PTA from Crude Terephthalic Acid?

    Polyester-grade PTA is defined by compliance with ASTM D788, which establishes test methods and specification limits for 4-carboxybenzaldehyde (4-CBA), p-toluic acid, colour, ash, and moisture. The 4-CBA concentration is the most restrictive purity parameter. In PTA, 4-CBA is held at or below 25 mg/kg, whereas crude oxidation product may contain 500–3,000 mg/kg depending on reactor configuration. 4-CBA is a monofunctional aldehyde impurity; during esterification with ethylene glycol it can terminate linear chain growth and generate colour-forming conjugated species. p-Toluic acid is controlled to 150 mg/kg maximum because it contains a single carboxylic acid group and acts as a polymer chain end without contributing to the diester backbone. Moisture is limited to ≤ 0.2 wt% because excess water in the feed shifts the esterification equilibrium and increases the thermal load on the esterification train. Ash is limited to ≤ 15 mg/kg to prevent catalyst inhibition and haze in bottle-grade PET. Colour is specified by the CIE b* coordinate, typically ≤ 1.5–2.0, measured per ISO 11664-4.

    Crude terephthalic acid produced from p-xylene oxidation carries 4-CBA, p-toluic acid, and coloured intermediates. Catalytic hydrogenation of the aqueous crude terephthalic acid slurry reduces 4-CBA to p-toluic acid, which is less chromophoric but still monofunctional; subsequent crystallisation and solid-liquid separation reduce p-toluic acid to the polyester-grade limit. The difference between PTA and crude terephthalic acid is therefore not only concentration but also the removal of aldehyde functional groups that disrupt linear polycondensation. Medium-purity terephthalic acid may be produced by stopping purification at a higher 4-CBA threshold for applications that do not require polyester-grade clarity or chain length. Published data for this specific configuration is limited, but the functional distinction is the monofunctional aldehyde content.

    Parameter Typical polyester-grade limit Test method
    Total acidity / purity ≥ 99.8 wt% ASTM D788
    4-CBA ≤ 25 mg/kg ASTM D788 HPLC-UV
    p-Toluic acid ≤ 150 mg/kg ASTM D788
    Water ≤ 0.2 wt% ASTM E203
    Ash ≤ 15 mg/kg ASTM D788 or ASTM D5630
    b* colour ≤ 1.5–2.0 ISO 11664-4

    In continuous PET slurry feed systems, particle-size distribution is monitored because fines content affects dust generation, bulk density, and feed-rate stability. Laser diffraction per ISO 13320:2020 reports D10, D50, and D90 values; sieving per ISO 2591-1 is used as a plant-level check. Specifications for polyester-grade PTA often restrict the sub-45 µm fraction and retain the median size near 100–130 µm, but published numeric limits for this specific configuration are limited because suppliers adjust distributions to the receiver design. Fines below 45 µm concentrate in dust collectors and increase baghouse cleaning frequency. Oversize agglomerates above 250 µm reduce dissolution rate in ethylene glycol and may pass unreacted into first-stage esterification. In dense-phase pneumatic conveying, variations in bulk density shift gravimetric feeder calibration. Continuous plants therefore compare incoming lot density against the baseline used for the rotary valve and loss-in-weight feeders; deviations greater than 5% require recalibration to maintain the EG:PTA molar ratio.

    Polyester Condensation Kinetics and Feedstock Purity Requirements

    In the melt-phase polymerisation sequence, PTA reacts with ethylene glycol in a two-step process. In esterification, PTA and ethylene glycol are charged at molar ratios near 1.15–1.4 EG:PTA and held at 260–280 °C and 1.0–2.0 bar in continuous stirred-tank reactors. The reaction produces bis(2-hydroxyethyl) terephthalate and water; the carboxylic acid groups autocatalyse the esterification, and no separate esterification catalyst is required. The mixture then enters the polycondensation stage at 275–290 °C and pressures below 1 mbar, catalysed by antimony trioxide, antimony acetate, or titanium alkoxide.

    Impurity effects are kinetic as well as stoichiometric. 4-CBA has one carboxylic acid group and one aldehyde group; after esterification the chain end is non-terephthaloyl and cannot propagate linear PET. Residual 4-CBA above 25 mg/kg suppresses the attainable degree of polymerisation and increases terminal carboxyl content. p-Toluic acid similarly introduces a non-reactive terminal group and reduces intrinsic viscosity per ASTM D4603. Metal ash above 15 mg/kg can interfere with catalyst selectivity and contribute to yellowing during melt processing. In five-reactor continuous PET trains, the pre-polycondensation vessel operates near 10–20 mbar and the finishing vessel near 0.5–1.5 mbar. Intrinsic viscosity targets of 0.60–0.65 dL/g for textile fibre and 0.80–0.85 dL/g for bottle-grade preforms are common; solid-state polymerisation is used after melt polymerisation for higher values. Residual 4-CBA and p-toluic acid reduce the rate of intrinsic viscosity build because each monofunctional impurity consumes a chain end that would otherwise react with bis(2-hydroxyethyl) terephthalate. Metal ash, especially iron and cobalt, accelerates thermal degradation at 280–290 °C and raises the concentration of acetaldehyde in bottle preforms. PTA quality therefore controls not only initial melting behaviour but also downstream acetaldehyde generation.

    When PTA Replaces Dimethyl Terephthalate in Melt-Phase Esterification

    PTA differs from dimethyl terephthalate in the volatile by-product formed during monomer preparation. Dimethyl terephthalate transesterification releases methanol, while PTA esterification releases water. This difference simplifies continuous PET plants because methanol recovery and distillation capacity is not required and the water by-product can be returned to the process or treated as lower-hazard effluent. The esterification of PTA and ethylene glycol is slower than transesterification of dimethyl terephthalate under identical temperature, but it eliminates the methanol recovery step and reduces the glycol excess. PTA also requires strict purification because aldehyde impurities such as 4-CBA are less volatile than the methyl ester impurities in dimethyl terephthalate and remain in the final polymer. Published data for this specific configuration is limited, but the shift from dimethyl terephthalate to PTA is well established in polyester manufacturing literature.

    Bulk Handling, Safety Boundaries, and Regulatory Classification

    Because PTA dust forms combustible atmospheres, handling systems require grounding, inerting, and deflagration venting in accordance with NFPA 652 and NFPA 654. Dust explosion severity parameters should be determined by ASTM E1226 or ISO 6184-1 on the specific lot because particle-size distribution and moisture affect explosion pressure. Avoid open flames and contact with strong oxidizers. PTA stored in dry silos below 60% RH does not require pre-drying; above this humidity, moisture pick-up can exceed the 0.2 wt% specification and interfere with esterification mass balance. For regulatory compliance, PTA is covered under REACH and national chemical inventories; food-contact PET made from PTA is regulated at the polymer level under FDA 21 CFR 177.1630 or EU No 10/2011, depending on jurisdiction.

    How Do PTA Grades Differ by End-Use Application?

    Suppliers may report the same base purity but adjust particle-size distribution, colour, and trace-metal limits for fibre, film, and bottle-grade PET. Fibre-grade PTA tolerates slightly higher colour and haze because fibre drawing does not require bottle-grade clarity, while bottle-grade PTA requires tight ash and b* limits to ensure low reheat and high transparency. Film-grade PTA combines low agglomerate content with controlled fines to avoid surface defects in biaxially oriented film. Table 2 summarises the main product distinctions among crude terephthalic acid, polyester-grade PTA, and medium-purity terephthalic acid.

    Product 4-CBA status p-Toluic acid status Colour Typical downstream use
    Crude terephthalic acid 500–3,000 mg/kg, oxidation-liquor dependent 400–2,000 mg/kg Yellow to brown Hydrogenation feedstock for PTA production
    Medium-purity terephthalic acid Above PTA limit; supplier-specific Above PTA limit; supplier-specific Off-white Non-PET applications or controlled blending; published data for this specific configuration is limited
    Purified terephthalic acid ≤ 25 mg/kg ≤ 150 mg/kg White PET resin, polyester fibre, and film